Physiochemical and mechanical characterisation of orthodontic 3D printed aligner material made of shape memory polymers (4D aligner material)

Islam Atta, Christoph Peter Bourauel, Yasmine Alkabani, Nesreen Mohamed, Hoon Kim, Abdulaziz Alhotan et al. · 2023 · 77 citationsRead the paper

All 8 authors

Ahmed A. M. Ghoneima, Tarek M. Elshazly

OBJECTIVES: To conduct a physiochemical and mechanical material analysis on 3D printed shape-memory aligners in comparison to thermoformed aligners. MATERIALS AND METHODS: Four materials were examined, including three thermoformed materials: CA Pro (CP), Zendura A (ZA), Zendura FLX (ZF), and one 3D printed material: Tera Harz (TC-85). Rectangular strips measuring 50 × 10 × 0.5 mm were produced from each material. Five tests were conducted, including differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA), shape recovery tests, three-points bending (3 PB), and Vickers surface microhardness (VH). RESULTS: DSC recorded glass transition temperatures (Tg) at 79.9 °C for CP, 92.2 °C for ZA, 107.1 °C for ZF, and 42.3 °C for TC-85. In DMA analysis at 20-45 °C, a prominent decrease in storage modulus was observed, exclusively for TC-85, as the temperature increased. Notably, within the temperature range of 30-45 °C, TC-85 exhibited substantial shape recovery after 10 min, reaching up to 86.1 %, while thermoformed materials showed minimal recovery (1.5-2.9 %). In 3 PB test (at 30, 37, 45 °C), ZA demonstrated the highest force at 2 mm bending, while TC-85 exhibited the lowest. Regarding VH at room temperature, there was a significant decrease for both ZA and ZF after thermoforming. ZA had the highest hardness, followed by ZF and TC-85, with CP showing the lowest values. CONCLUSIONS: TC-85 demonstrates exceptional shape memory at oral temperature, improving adaptation, reducing force decay, and enabling, together with its higher flexibility, extensive tooth movement per step. Additionally, it maintains microhardness similar to thermoformed sheets, ensuring the durability and effectiveness of dental aligners. CLINICAL RELEVANCE: The 3D printed aligner material with shape memory characteristics (4D aligner) has revolutionized the orthodontic aligner field. It showed mechanical properties more suitable for orthodontic treatment than thermoforming materials. Additionally, it offers enhanced control over aligner design and thickness, while optimizing the overall workflow. It also minimizes material wastage, and reduces production expenses.

What the full text shows

Working prototype
  • TC-85 exhibited significantly higher shape recovery at oral temperatures compared to thermoformed materials. — 86.1% recovery at 45 °C, 54.9% at 37 °C, and 8.4% at 30 °C vs. 1.5-2.9% for thermoformed materials (10 min immersion in water bath after 180° bending)
  • TC-85 has a glass transition temperature (Tg) within a range that allows activation at oral temperatures. — Tg = 42.3 °C (DSC curve starts at 30.4 °C) vs. 79.9-107.1 °C for thermoformed materials (DSC analysis from -40 °C to 240 °C)
  • TC-85 showed a prominent decrease in storage modulus as temperature increased. — Storage modulus ranged from 100 MPa to 3000 MPa (DMA analysis at 20-45 °C)
  • TC-85 exhibited the lowest force during three-point bending tests. — Lowest force at 2 mm bending (Tested at 30, 37, and 45 °C)
  • TC-85 maintains surface microhardness comparable to thermoformed sheets. — 8.1 ± 0.9 VH (Vickers microhardness at room temperature)
Setup
Four materials: CA Pro, Zendura A, Zendura FLX (thermoformed), and Tera Harz TC-85 (DLP 3D printed).
How
The study compared one 3D printed material (TC-85) with three thermoformed materials (CP, ZA, ZF) using DSC, DMA, shape recovery tests, three-point bending, and Vickers microhardness. Specimens were prepared as rectangular strips (50 x 10 x 0.6 mm).