Mechanical properties of modern restorative “bioactive” dental materials - an in vitro study
Mateusz Radwański, Ewa Zmysłowska-Polakowska, Karolina Osica, Michał Krasowski, Salvatore Sauro, Louis Hardan et al. · 2025 · 27 citationsRead the paper
All 7 authors
Monika Łukomska−Szymańska
This study aimed at assessing the mechanical properties and degradation of commercial bioactive materials. The bioactive materials (Activa Bioactive Restorative, Beautifil Flow Plus F00, F03, Predicta Bulk Bioactive) and composite resin Filtek Supreme Flow were submitted to flexural and diametral tensile strength tests (FS, DTS), modulus of elasticity (ME) evaluation, and analysis of aging in 70% ethanol and saliva on their hardness and sorption. The results for DTS ranged from 33.16 MPa (Beautifil Flow Plus F03) to 47.74 MPa (Filtek Supreme Flow). The highest FS was 120.40 MPa (Predicta Bulk Bioactive), while the lowest values were 86.55 MPa (Activa Bioactive Restorative). Activa Bioactive Restorative showed the lowest ME, as well as the highest water sorption both in alcohol and artificial saliva. Moreover, aging in saliva induced a significant decrease in hardness for Activa Restorative (p < .01). Alcohol storage caused a significant decrease in hardness for all materials (p < .0001). All tested materials met the basic requirements for light-curing materials in terms of DTS and FS. However, all materials showed higher sorption in alcohol than in saliva, while hardness decreased significantly after 30 days. Predicta Bulk Bioactive presented the highest mechanical parameters, initial hardness, and the lowest sorption of alcohol and saliva.
What the full text shows
Shown in the lab- Predicta Bulk Bioactive exhibited the highest flexural strength (FS) and modulus of elasticity (ME). — FS: 120.40 MPa; ME: 7.27 GPa (Three-point bending test)
- Filtek Supreme Flow exhibited the highest diametral tensile strength (DTS). — 47.74 MPa (Cylindrical specimens)
- Activa Bioactive Restorative showed the highest water sorption after 30 days. — 106.49 µg/mm³ in alcohol; 46.27 µg/mm³ in saliva (30-day incubation at 37 °C)
- Alcohol storage caused a significant decrease in hardness for all tested materials. — p < .0001 (30-day immersion in 70% ethanol)
- Activa Bioactive Restorative exhibited the lowest flexural strength and modulus of elasticity. — FS: 86.55 MPa; ME: 3.45 GPa (Three-point bending test)
- All tested materials met the minimum ADA and ISO requirements for DTS and FS. — DTS > 24 MPa; FS > 80 MPa (Light-curing resin-based materials)
- Setup
- Five materials (Activa Bioactive Restorative, Beautifil Flow Plus F00, Beautifil Flow Plus F03, Predicta Bulk Bioactive, and Filtek Supreme Flow) with sample sizes of 9-20 specimens per group depending on the test.
- How
- The study performed three-point bending tests for FS and ME, cylindrical tests for DTS, and immersion tests in 70% ethanol and artificial saliva to measure sorption and Vickers hardness over 30 days. Statistical analysis included Kruskal-Wallis, Welch's t-test, and repeated measures ANOVA.
- Limitations
- In vitro study (not in vivo) · Limited to 30-day aging period · Small sample size per group (n=9 to 20)
Summarized by Gemma 4 from the open-access full text · 8 Oct 2026. Read it