Mechanical and viscoelastic properties of a temperature-responsive photocurable resin for 3D printed orthodontic clear aligners

Jin Young Choi, Hoon Kim, Seong Hun Kim, Su Jung Kim, Jung‐Yul Cha, Se Yeon Lee et al. · 2025 · 28 citationsRead the paper

All 12 authors

Jiho Lee, Jinhong Min, Sunho Jang, Tanveer Ahmed Khan, Hyun‐Joong Kim, Ki Beom Kim

This study investigates the mechanical and viscoelastic properties of TC-85, a biocompatible material specifically designed for orthodontic applications, with a focus on how temperature variations influence its mechanical and viscoelastic properties and their relevance to clinical outcomes. Using a Digital Light Processing (DLP) 3D printer, the photosensitive resin TC-85 is printed, and extensive thermo-mechanical testing is conducted, which includes evaluations of tensile modulus, stress relaxation, and creep behavior. Dynamic Mechanical Analysis (DMA) is conducted at temperatures varying from 30 to 45 °C to assess the material's adaptive response to thermal fluctuations. TC-85 is distinguished by its unique mechanical properties, which include a temperature-sensitive stiffness, stress relaxation capability, and shape memory feature. The results demonstrate that TC-85 maintains an enhanced level of residual force and a faster recovery of strain through numerous cycles of loading and unloading. At 40 °C, TC-85 displays a substantial reduction in its storage modulus, while maintaining consistent strain recovery and volumetric constancy. The study highlights TC-85's potential in orthodontic treatments, providing adaptable mechanical and viscoelastic properties that enable the exertion of consistent and regulated forces on teeth. Its resistance to force decay, stable volume at raised temperatures, and shape memory properties enhance hygienic maintenance and patient comfort, positioning TC-85 as a pioneering material for the next generation of clear aligners.

What the full text shows

Shown in the lab
  • Shape recovery rate increases with temperature, reaching near-complete recovery at the highest tested temperature. — 99% recovery at 45 °C vs. 34.4% at 30 °C (after 60 min) (Bending test on specimens 0.5 mm to 0.7 mm thickness)
  • Strain recovery improves significantly at higher temperatures after repeated loading cycles. — >90% recovery rate at 45 °C vs. <80% at 30 °C and 35 °C (13 cycles of 2% elongation held for 60 min followed by 60 min release)
  • Storage modulus decreases as temperature rises, with a plateau effect after 40 °C. — Distinct decrease from 30 °C to 40 °C; no significant change beyond 40 °C (DMA frequency sweep (0.1 to 100 Hz))
  • Tensile strength and elastic modulus decrease as temperature increases, regardless of specimen thickness. — Gradual decrease from 30 °C to 45 °C (Specimen thicknesses of 0.5 mm, 0.65 mm, and 0.8 mm)
  • Maximum standard force at 20% strain is thickness-dependent at low temperatures but becomes independent at higher temperatures. — Difference diminished and became non-significant beyond 40 °C (Comparison of 0.5 mm, 0.65 mm, and 0.8 mm thicknesses)
Setup
TC-85 photocurable resin; specimens printed at thicknesses of 0.5, 0.65, and 0.8 mm; tested at temperatures of 30, 35, 40, and 45 °C.
How
TC-85 resin was 3D printed via DLP and post-cured. Mechanical properties were evaluated using tensile testing, Dynamic Mechanical Analysis (DMA) for storage/loss modulus and stress relaxation, and a U-shaped bending test for shape memory.
Limitations
Results may differ under 100% humidity (oral cavity conditions) due to polyurethane water absorption. · Stress relaxation tests were limited to 60-minute intervals, whereas actual aligner wear exceeds 24 hours.